The effect of water vapor on selective oxidation of Fe–Cr alloys E Essuman, GH Meier, J Żurek, M Hänsel, WJ Quadakkers Oxidation of metals 69 (3), 143-162, 2008 | 205 | 2008 |
Anomalous temperature dependence of oxidation kinetics during steam oxidation of ferritic steels in the temperature range 550–650 C J Żurek, E Wessel, L Niewolak, F Schmitz, TU Kern, L Singheiser, ... Corrosion science 46 (9), 2301-2317, 2004 | 177 | 2004 |
Growth and adherence of chromia based surface scales on Ni-base alloys in high-and low-pO2 gases J Zurek, DJ Young, E Essuman, M Hänsel, HJ Penkalla, L Niewolak, ... Materials Science and Engineering: A 477 (1-2), 259-270, 2008 | 165 | 2008 |
Enhanced internal oxidation as trigger for breakaway oxidation of Fe–Cr alloys in gases containing water vapor E Essuman, GH Meier, J Żurek, M Hänsel, L Singheiser, WJ Quadakkers Scripta materialia 57 (9), 845-848, 2007 | 141 | 2007 |
Steam oxidation of ferritic steels–laboratory test kinetic data WJ Quadakkers, PJ Ennis, J Zurek, M Michalik Materials at high temperatures 22 (1-2), 47-60, 2005 | 101 | 2005 |
Effect of water vapor on high-temperature oxidation of FeCr alloys WJ Quadakkers, J Żurek, M Hänsel Jom 61 (7), 44-50, 2009 | 85 | 2009 |
The effect of water-vapor content and gas flow rate on the oxidation mechanism of a 10% Cr-ferritic steel in Ar-H 2 O mixtures J Żurek, M Michalik, F Schmitz, TU Kern, L Singheiser, WJ Quadakkers Oxidation of metals 63 (5), 401-422, 2005 | 85 | 2005 |
Effect of water vapour on growth and adherence of chromia scales formed on Cr in high and low pO2-environments at 1000 and 1050 C M Michalik, M Hänsel, J Zurek, L Singheiser, WJ Quadakkers Materials at High Temperatures 22 (3-4), 213-221, 2005 | 80 | 2005 |
Protective and non-protective scale formation of NiCr alloys in water vapour containing high-and low-pO2 gases E Essuman, GH Meier, J Zurek, M Hänsel, T Norby, L Singheiser, ... Corrosion Science 50 (6), 1753-1760, 2008 | 78 | 2008 |
Temperature dependence of oxide scale formation on high-Cr ferritic steels in Ar–H2–H2O DJ Young, J Zurek, L Singheiser, WJ Quadakkers Corrosion Science 53 (6), 2131-2141, 2011 | 74 | 2011 |
Development of high chromium ferritic steels strengthened by intermetallic phases B Kuhn, M Talik, L Niewolak, J Zurek, H Hattendorf, PJ Ennis, ... Materials Science and Engineering: A 594, 372-380, 2014 | 69 | 2014 |
Viewing information collection system and method using data braodcasting, and broadcast receiver, viewing information server, shop terminal, and advertiser terminal used therein H Tatsumi, E Ueda US Patent App. 10/096,824, 2002 | 54 | 2002 |
Oxidation in steam and steam/hydrogen environments WJ Quadakkers, J Żurek Elsevier, 2010 | 50 | 2010 |
Microstructural stability and oxidation behavior of Sanicro 25 during long‐term steam exposure in the temperature range 600–750° C J Zurek, SM Yang, DY Lin, T Hüttel, L Singheiser, WJ Quadakkers Materials and corrosion 66 (4), 315-327, 2015 | 42 | 2015 |
Basic creep models for 25Cr20NiNbN austenitic stainless steels R Sandström, M Farooq, J Zurek Materials Research Innovations 17 (5), 355-359, 2013 | 29 | 2013 |
Effect of specimen thickness on the growth rate of chromia scales on Ni-base alloys in high-and low-pO2 gases J Zurek, GH Meier, E Essuman, M Hänsel, L Singheiser, WJ Quadakkers Journal of alloys and compounds 467 (1-2), 450-458, 2009 | 29 | 2009 |
Steam oxidation of 9% to 12% Cr steels: critical evaluation and implications for practical application J Zurek, E De Bruycker, S Huysmans, WJ Quadakkers Corrosion 70 (2), 112-129, 2014 | 26 | 2014 |
Effect of oxygen partial pressure on the oxidation behaviour of an yttria dispersion strengthened NiCr-base alloy E Essuman, GH Meier, J Zurek, M Hänsel, L Singheiser, T Norby, ... Journal of materials science 43 (16), 5591-5598, 2008 | 19 | 2008 |
Why the growth rates of alumina and chromia scales on thin specimens differ from those on thick specimens WJ Quadakkers, P Huczkowski, D Naumenko, J Zurek, GH Meier, ... Materials Science Forum 595, 1111-1118, 2008 | 18 | 2008 |
Effect of alloying additions in ferritic 9-12% Cr steels on the temperature dependence of the steam oxidation resistance J Zurek, L Nieto Hierro, J Piron-Abellan, L Niewolak, L Singheiser, ... Materials Science Forum 461, 791-798, 2004 | 12* | 2004 |