Calorimetric study of amorphization in planar, binary, multilayer, thin-film diffusion couples of Ni and Zr EJ Cotts, WJ Meng, WL Johnson Physical review letters 57 (18), 2295, 1986 | 180 | 1986 |
Corrosion resistant PEM fuel cell Y Li, WJ Meng, S Swathirajan, SJ Harris, GL Doll US Patent 5,624,769, 1997 | 174* | 1997 |
Mechanical properties of Ti-containing and W-containing diamond-like carbon coatings WJ Meng, BA Gillispie Journal of applied physics 84 (8), 4314-4321, 1998 | 167 | 1998 |
Epitaxial growth of aluminum nitride on Si (111) by reactive sputtering WJ Meng, J Heremans, YT Cheng Applied physics letters 59 (17), 2097-2099, 1991 | 135 | 1991 |
Growth and mechanical anisotropy of TiN thin films WJ Meng, GL Eesley Thin Solid Films 271 (1-2), 108-116, 1995 | 122 | 1995 |
Growth of aluminum nitride thin films on Si (111) and Si (001): Structural characteristics and development of intrinsic stresses WJ Meng, JA Sell, TA Perry, LE Rehn, PM Baldo Journal of Applied Physics 75 (7), 3446-3455, 1994 | 121 | 1994 |
Tribology of metal-containing diamond-like carbon coatings SJ Harris, AM Weiner, WJ Meng Wear 211 (2), 208-217, 1997 | 113 | 1997 |
Maximum thickness of amorphous NiZr interlayers formed by a solid‐state reaction technique WJ Meng, CW Nieh, WL Johnson Applied physics letters 51 (21), 1693-1695, 1987 | 107 | 1987 |
Structure and mechanics of W-DLC coated spur gears JC Jiang, WJ Meng, AG Evans, CV Cooper Surface and coatings technology 176 (1), 50-56, 2003 | 105 | 2003 |
Mechanical properties and microstructure of TiC/amorphous hydrocarbon nanocomposite coatings WJ Meng, RC Tittsworth, LE Rehn Thin Solid Films 377, 222-232, 2000 | 86 | 2000 |
Fabrication, assembly, and testing of Cu-and Al-based microchannel heat exchangers F Mei, PR Parida, J Jiang, WJ Meng, SV Ekkad Journal of Microelectromechanical systems 17 (4), 869-881, 2008 | 85 | 2008 |
Characterization of microstructure and mechanical behavior of sputter deposited Ti-containing amorphous carbon coatings B Feng, DM Cao, WJ Meng, J Xu, RC Tittsworth, LE Rehn, PM Baldo, ... Surface and Coatings Technology 148 (2-3), 153-162, 2001 | 83 | 2001 |
Solid state interdiffusion reactions of Ni/Zr diffusion couples WJ Meng, CW Nieh, E Ma, B Fultz, WL Johnson Materials Science and Engineering 97, 87-91, 1988 | 82 | 1988 |
Effect of alloying elements on the γ’antiphase boundary energy in Ni-base superalloys M Dodaran, AH Ettefagh, SM Guo, MM Khonsari, WJ Meng, N Shamsaei, ... Intermetallics 117, 106670, 2020 | 81 | 2020 |
Strain effects in epitaxial GaN grown on AlN‐buffered Si (111) WJ Meng, TA Perry Journal of Applied Physics 76 (12), 7824-7828, 1994 | 81 | 1994 |
Hydrogen‐induced crystal to glass transformation in Zr3Al WJ Meng, PR Okamoto, LJ Thompson, BJ Kestel, LE Rehn Applied physics letters 53 (19), 1820-1822, 1988 | 76 | 1988 |
Friction and wear characteristics of ceramic nanocomposite coatings: Titanium carbide/amorphous hydrocarbon DM Cao, B Feng, WJ Meng, LE Rehn, PM Baldo, MM Khonsari Applied Physics Letters 79 (3), 329-331, 2001 | 75 | 2001 |
Mechanical failure of metal/ceramic interfacial regions under shear loading X Zhang, B Zhang, Y Mu, S Shao, CD Wick, BR Ramachandran, WJ Meng Acta Materialia 138, 224-236, 2017 | 70 | 2017 |
Overview: additive manufacturing enabled accelerated design of Ni-based alloys for improved fatigue life S Shao, MM Khonsari, S Guo, WJ Meng, N Li Additive Manufacturing 29, 100779, 2019 | 69 | 2019 |
Mechanical, thermal, and corrosion properties of Cu-10Sn alloy prepared by laser-powder-bed-fusion additive manufacturing C Zeng, B Zhang, AH Ettefagh, H Wen, H Yao, WJ Meng, S Guo Additive Manufacturing 35, 101411, 2020 | 67 | 2020 |